Zinc Aluminium metalizing wire is manufactured by ultra-pure electrolytic zinc and aluminium. They are appropriate for flame spray and electric arc alloy spraying. Their pureness matches 2.3 – zinc aluminium wires for thermic spraying, Through the EN ISO 14919 standard.
Adopting a coating should be made precisely because it will decide the status of your work and forward the lifetime of your project. We have the information, experience, and quality of products that make it the perfect companion to make your choice easy.
We are a zinc aluminium metalizing wire manufacturer in India for thermal spray coating. Zinc Aluminium metalizing wire is a corrosion-resistant element in a non-oxidizing environment; usually used to provide resistance to neutral climatic conditions and seawater ecosystems. We also manufacture and supply metalizing gun, metalizing wire, zinc spray gun, flame spray gun, arc spray gun, thermal spray gun, sand blasting cabinet, sand blasting machine, Shot blasting machine, Sand blasting hopper, and abrasive shots like abrasive garnet, copper slag, steel shots, cut wire shots. Before thermal spray coating blasting is done for surface roughness.
We are a zinc aluminium metalizing wire supplier and exporter in India. We maintain metalizing wire and alloy wires quality and provide the best services. We also manufacture and supply metalizing gun, metalizing wire, zinc spray gun, flame spray gun, arc spray gun, thermal spray gun, sand blasting cabinet sand blasting machine, Shot blasting machine, Sand blasting hopper, and abrasive shots like abrasive garnet, copper slag, steel shots, cut wire shots. Before thermal spray coating blasting is done for surface roughness.
Typical Values | DIN EN ISO 14919 | |
Zn | 84-86 % | 84-86 % |
Al | 14-16 % | 14-16 % |
Other Elements | ||
Pb | ≤0.003 % | ≤0.007 % |
Cd | ≤0.001 % | ≤0.004 % |
Pb+Cd | ≤0.004 % | ≤0.011 % |
Sn | ≤0.001 % | ≤0.001% |
Fe | ≤0.015 % | ≤0.02 % |
Cu | ≤0.002 % | ≤0.01 % |
Si | ≤0.01 % | ≤0.12 % |
Other Total | ≤0.03 % | ≤0.17 % |
Tensile Strength Rm | 110-150 | MPa |
Yield Point Rp0.2 | 80-130 | MPa |
Elongation A100mm | Min 50 | % |
Density | ~ 5.73 | g/cm3 |
Melting Range | ~ 382-450 | °C |